物理指标
名称
|
测试方法
|
FST-P90
|
FST-P100
|
FST-P110
|
FST-P120
|
FST-P130
|
外观
|
目测
|
颗粒
|
颗粒
|
颗粒
|
颗粒
|
颗粒
|
软化点℃
|
环球法
GB/T4507
|
90-100
|
100-110
|
110-120
|
120-130
|
130-135
|
色号#
|
ASTMD-1544
|
≤4
|
≤4
|
≤4
|
≤4
|
≤4
|
熔融粘度
(200℃ )mpa.s
|
ASTMD-3236
|
≤500
|
≤500
|
≤500
|
≤500
|
≤500
|
酸值(mgKOH/g
|
GB2895
|
≤0.5
|
≤0.5
|
≤0.5
|
≤0.5
|
≤0.5
|
溴值gBr /100g
|
HG2231-91-A
|
30-50
|
30-50
|
30-50
|
30-50
|
30-50
|
比重(g/cm3)
|
ASTM D71-72A
|
0.96-0.98
|
0.96-0.98
|
0.96-0.98
|
0.96-0.98
|
0.96-0.98
|
灰分VOI%
|
ETM-E-99
|
0.03Max
|
0.03Max
|
0.03Max
|
0.03Max
|
0.03Max
|
蜡雾点℃
|
ASTD2500
|
Max138
|
Max138
|
Max138
|
Max138
|
Max138
|